Mould Repair by Laser

Of the ten typical defects found on moulds and dies, nearly all are local and can be repaired by laser build-up welding directly on the tool. A die-casting die with heat-checking on the cavity surface arrives in the toolroom late on Friday. The press stands ready, but production cannot resume until the defect is fixed. The toolmaker’s first step is not to assess the look of the damage, but to identify the steel grade and its heat treatment. This decision guides the entire repair process. 

Most defects are local and can be welded in place

Damage on injection moulds and die-casting dies is usually confined to specific areas. The main groups are:

  • Edges: chipped or worn parting-line edges, worn sealing and shut-off edges, worn radii and corners
  • Cracks: heat-checking cracks on die-casting surfaces (surface only), short cracks at edges
  • Erosion and pitting: erosion and pitting from the melt, local surface loss
  • Seats and dents: damaged ejector or insert seats, dents from handling

Nearly all of these can be repaired by laser build-up welding directly on the tool. Only through-cracks that run across the entire insert require a new part. For all others, material is added where needed and the tool remains in one piece.

Laser beam build-up welding restores surface without affecting hardness or dimensions

Laser beam build-up welding adds filler wire, matched to the tool steel, at the precise spot indicated by the microscope cross-hair. The process uses pulse energy up to 170 J and peak power up to 13 kW, allowing controlled melting of the filler without significant heating of the surrounding steel. This keeps the tool’s hardness and dimensions intact. Mobile five-axis workstation systems are brought to the mould, whether in the toolroom or next to the press. Swivelling optics reach undercuts and deep cavities, so most repairs do not require dismantling or transport of the tool.

The steel grade as decisive factor of repair

The first step in any repair is to identify the steel grade, such as 1.2344 (H13) or 1.2343, and its heat treatment. Filler wire, pulse shape and any pre-heating are chosen to match the material. High-carbon tool steels are prone to cracking under heat. Super Pulse Technology shapes the pulse to keep the heat-affected zone small, allowing even those steels to be welded without cracks. “In the toolroom people judge a defect by how it looks, but the steel decides the route. I have seen two defects that looked identical and needed completely different settings,” says Alexander Bellouzi, Senior Design & Engineering at Sigma Laser. 

More Information

(Source: Sigma Laser GmbH)

Schlagworte

AutomationCladdingHeat CracksLaserLaser Beam Build-up WeldingLaser Beam WeldingMouldsSteelWeldingWelding Wire

Verwandte Artikel

17.11.2026

EWM: Why Many Automation Projects Fail at the Preparation Stage

In its new eBook, EWM highlights the typical pitfalls, explains which technical aspects are crucial and outlines how to get started successfully.

Automated Welding Automation Cobot EBook Feasibility Study Material Behaviour Robot Skills Welding Welding Task
Read more
17.11.2026

Formnext 2026: Nippon Sanso introduces 3DPro RotoTIG

Nippon Sanso will showcase the 3DPro RotoTIG torch in Europe at Formnext 2026, presenting a new approach to wire-based metal additive manufacturing.

Additive Manufacturing AM Cladding Electrode Tungsten Welding Welding Wire Wire-based Metal Additive Manufacturing
Read more
15.11.2026

One Helmet for the Entire Work Process

Thanks to innovative slide-up technology, welders can switch between welding, grinding and cutting with a single motion - without having to remove the helmet.

Cutting Grinding Personal Protective Equipment PPE Respiratory Protection Welding Welding Helmet Welding Mode Workplace Safety
Read more
13.11.2026

Fakuma 2026 Signals Shift Toward Integrated Manufacturing Solutions

Hymson Novolas has concluded its participation in Fakuma 2026, the 30th international trade fair for plastics processing where discussions showed that requirements for la...

Automation FAKUMA Handheld Laser Beam Welding Joining Plastics JP LBW Plastics Plastics Welding Radial Welding Trade Fair
Read more
f. l. t. r.: Arc Cup participants Timo Clasen, Lucas Hammerschmidt and Tim von Trzebiatowski, Jürgen Raun, welding instructor at HWK Flensburg training centre (front), participant Alexander Graf and Ronald Pajuelo, Chairman of the DVS national working group
12.11.2026

Jugend Schweißt Winners Receive Medals at Arc Cup in China

At the international welding competition Arc Cup in China, the German team impressed with its performance and took home silver and bronze medals.

Arc Cup DVS DVS Group Gas Welding German Welding Society Jugend schweißt Magnesium Manual Arc Welding Metal Active Gas Welding TIG Welding Young Welders Competition
Read more